I have a Durometer, a swedish machine for HRC testing a very good machine :).
Why i ask is, i have heard that the optimum hardnes for O1 is 61-62 HRC and that it will hold up with very thin edge with that hardnes. But i doubt that. I like O1 and use it very much, but i doubt that it is...