Danneskjold
Member
Hi again!
Thanks for the help on the last problem. It seems that thinking annealing the knife was a better substitute for normalizing did cause the cracking problems.
This next problem I have had for a while. (Sorry if this is the wrong section.)
I electro etch my knife using a home made etcher done from Red Beard Op's design. I buy stencils from TUS Technologies. I just dump a bit of table salt into a bowl and put warm water over it. Don't measure any ratios, just wing it. I used to use a brass marker + felt, but I switched to using disposable Q-Tips. It seems to give me better control and accuracy. Both gave me the same problem.
The problem isn't the corrosion.
The problem is that the corrosion bleeds through for ~3 days or so. I.E. If I clean it off now, it'll still come out in a few days.
Am I doing something wrong? Should I be getting stencils from somewhere else? These ones seem rather thin and I get a lot of moisture bleed through to the back side of the stencil. Should I get some dedicated etching fluid?
Thanks for the help on the last problem. It seems that thinking annealing the knife was a better substitute for normalizing did cause the cracking problems.
This next problem I have had for a while. (Sorry if this is the wrong section.)
I electro etch my knife using a home made etcher done from Red Beard Op's design. I buy stencils from TUS Technologies. I just dump a bit of table salt into a bowl and put warm water over it. Don't measure any ratios, just wing it. I used to use a brass marker + felt, but I switched to using disposable Q-Tips. It seems to give me better control and accuracy. Both gave me the same problem.
The problem isn't the corrosion.
The problem is that the corrosion bleeds through for ~3 days or so. I.E. If I clean it off now, it'll still come out in a few days.
Am I doing something wrong? Should I be getting stencils from somewhere else? These ones seem rather thin and I get a lot of moisture bleed through to the back side of the stencil. Should I get some dedicated etching fluid?