Danneskjold
Member
Hi again!
I've got a project coming up where I'll be heat treating thin (~1/16") AEBL. But I'll be doing it in a propane forge.
Now, I don't need ultra-hard heat treatment, or cryogenic treatment. In fact, I'll be tempering pretty soft and springy. But heat treating it rather straight is a bit important. I do have anti-scale coating.
What process would you recommend? Thanks!
I've got a project coming up where I'll be heat treating thin (~1/16") AEBL. But I'll be doing it in a propane forge.
Now, I don't need ultra-hard heat treatment, or cryogenic treatment. In fact, I'll be tempering pretty soft and springy. But heat treating it rather straight is a bit important. I do have anti-scale coating.
What process would you recommend? Thanks!