I'm curious if anyone has any temps they go with for refining the grain in O-1 tool steel. I have been going a hair above austenizing temp say 1525, then air cool, back in at 1475, air cool and so forth dropping 50 degrees with each cycle down to 1275. Once done cycling the steel I go back in at 1450 for 10 min to Austenize then quench. I have been getting good results, but I'm kinda flying by the seat of my pants on these temps. Does my process sound about right? Anyone who has a lot of experience with O-1 tool steel on here who can point me in the right direction. I haven't used a whole lot of it myself and want to make sure I'm getting the most out of it that I can. Thanks!