Hey guys......I just finished forging 3 billets of layer damascus from 24 in circular saw blade material <L6?> and 15n20.......everything welded up fine but I ended up with extremely hard forge scale on the surface of the billets.......I am wondering what is causing this as I was fluxing entire billet during weld....this is the first time that I have tried the circular saw blade in damascus but i have forged it into knives by itself and not had a scale problem.......any thoughts of why this is happening ????