Well-Known Member
I have a set of 1084 blades that are in need of stress relief prior to heat treat. I plan on foil wrapping them to minimize carbonization, as my blade tolerances don't allow for much more steel to be removed following heat treat. To relieve stress, I follow a three step process of bringing the blade to critical temperature, letting it soak for five minutes, and cooling it in air as the blade color changes from red to black. I am new to foil wrapping, and am unsure how how the blade would be cooling in the foil wrap. Can I assume the blade is cool as the wrap cools, or should I give it more time for the blade inside to cool before I repeat the process? Thanks for your help!