Hi guys,
So my first batch of aeb-l knife are out for heat treat but i would like to make some blades in 80crv2 and HT by myself. With my CNC and my new 2x72 and bunch of other stuff, my budget is limited and i cant afford a kiln for the moment. So i was thinking buying a small propane forge with a thermometer.
So my question is, can i do proper heat treat with a setup like that ? I would like to go with 80crv2 because from what i read, its pretty easy to HT.
Thanks!
So my first batch of aeb-l knife are out for heat treat but i would like to make some blades in 80crv2 and HT by myself. With my CNC and my new 2x72 and bunch of other stuff, my budget is limited and i cant afford a kiln for the moment. So i was thinking buying a small propane forge with a thermometer.
So my question is, can i do proper heat treat with a setup like that ? I would like to go with 80crv2 because from what i read, its pretty easy to HT.
Thanks!