Hello all - I had Sandvik's 12C27 on my mind this morning, put in oven for 5 minute/blade at 1975ºF. After plate quenching I tested the blades and only had 52 RC. Hmmm, A good bit low I'm thinking - I was expecting more along the lines of 60+ Rc. I put blades in freezer for a -5ºF freeze (Sandvik says -5ºF is good for about 1 point, and -95ºF for 2 to 2.5 points) then remembered it was NOT 12C27, but 440C blades.
While Sandvik does NOT recommend re-heat treating any of the Sandvik steels, what about 440C - can it be annealed then re-heat treated? OR - does it even need to be annealed prior to re-heat treating?
Comments, suggestions, or guidance please,
Ken H> (Hey, getting old 'n forgetful is better than the alternative)
While Sandvik does NOT recommend re-heat treating any of the Sandvik steels, what about 440C - can it be annealed then re-heat treated? OR - does it even need to be annealed prior to re-heat treating?
Comments, suggestions, or guidance please,
Ken H> (Hey, getting old 'n forgetful is better than the alternative)