Here's my next 3 knives ground ready for Pin holes and pre HT hand sanding to fix a couple small wobbles in the grind lines. I wanted to try to make 3 knives from the same template but do each one a bit different from the next.
All are 10" OAL with 5" Blades
Top one is an almost full height hollow grind from 1/8" 440c
Middle one is about a 2/3 height hollow grind from 1/8" 440c added a swedge to this one.
Bottom one is also a 2/3 height hollow grind this one is from 3/16" 440c this one also has a swedge but gave this one a subtle recurve.
I want to try bolsters for the frist time on one of them, most likely the first one. I have some 1" x 3/4" nickle silver bar stock with pins of the same
comments or critiques welcomed and encouraged.
![10inchhunters.jpg](http://i1197.photobucket.com/albums/aa423/jason_leclair888/10inchhunters.jpg)
All are 10" OAL with 5" Blades
Top one is an almost full height hollow grind from 1/8" 440c
Middle one is about a 2/3 height hollow grind from 1/8" 440c added a swedge to this one.
Bottom one is also a 2/3 height hollow grind this one is from 3/16" 440c this one also has a swedge but gave this one a subtle recurve.
I want to try bolsters for the frist time on one of them, most likely the first one. I have some 1" x 3/4" nickle silver bar stock with pins of the same
comments or critiques welcomed and encouraged.