Thank you both for the suggestion of 1950F. I haven't been doing this long enough to question any of the temps. that have been recommended.
But I will try these temps. as well and log results for future reference.
Thank you again for your help,,,
retired
I am trying to make a spring for a slip joint folder out of ATS 34. I was given instructions to heat
treat at 1850deg. F and soak for 30min, I then air quenched and then was told to draw at 1160 deg. F
for 2hours one time. The result was 40RC. Could you possibly advise me on a procedure with an...