Guindesigns
Well-Known Member
Hey dogs, I've been working on two knives for my boss for some time now and the last time i worked on them was heat treating them. Now I having a problem i put hem to the side for a while trying to get my shop at my house up and running but I went to my mentors house and starting grinding on them and even with the kmg all the way up and a 80 trizac belt on I could on get the scale to come off the flats. Is there any way to make this easier without going to a lower grit?? and/or any little tricks to help losen the scale from the metal?? thank Dogs.
-Young Pup
p.s. sad thing was we had both knives in foil when we did the heat treat to stop the scale. but it burned up some how???:confused2::confused2: Now im stuck with Scale man I hate scale:sad::sad: why me. lol:31::52:
-Young Pup
p.s. sad thing was we had both knives in foil when we did the heat treat to stop the scale. but it burned up some how???:confused2::confused2: Now im stuck with Scale man I hate scale:sad::sad: why me. lol:31::52: