Gliden07
Well-Known Member
Well I sanded my knife blank down to 220 grit paper. All the file marks are gone. Need to heat treat now blade is 01 tool steel 1/8"x 1", plan on using oxy-acetelyne torch with a Rosebud tip and Canola oil for the quench. Question is should I pre-heat oil before quench? And how long should I quench? Thanks!
![20170602_195821.jpg 20170602_195821.jpg](https://knifedogs.com/data/attachments/42/42075-6b9ed51f12173cf3e49ffc217e90a289.jpg)
![20170602_195821.jpg 20170602_195821.jpg](https://knifedogs.com/data/attachments/42/42075-6b9ed51f12173cf3e49ffc217e90a289.jpg)
Last edited: