TJ Smith Well-Known Member Mar 14, 2013 #1 Just forged a billet out San-Mai type with 15n20 in the center and 1 layer chain on each side.Have a couple small lines that didn't weld. Any way to fix these? mig weld, what steel?, brass ,silver solder. Hate to waste the chain. Thanks TJ Smith
Just forged a billet out San-Mai type with 15n20 in the center and 1 layer chain on each side.Have a couple small lines that didn't weld. Any way to fix these? mig weld, what steel?, brass ,silver solder. Hate to waste the chain. Thanks TJ Smith
D Diamond G Knives Well-Known Member May 14, 2013 #2 Is the blade already ground? If not, Flux bring to welding heat then weld the cracks shut. Possibly grind them out and re forge? God Bless Mike
Is the blade already ground? If not, Flux bring to welding heat then weld the cracks shut. Possibly grind them out and re forge? God Bless Mike