So I haven't been happy with my stabilizing processes so far, I am trying to stabilize some Myrtle and have tried several methods, here is my question. What are the places like Knife and Gun using? Vacuum or Pressure or both? So I understand that the vacuum will take the air out but I would think after you are done your scales should sink in the solution, mine are not. I found a pressurized process using Alumilite but not sure how that stuff penetrates the wood. Seems like the best process would be to use both first the vacuum ant then cure it under pressure. Also make me wonder if they are using a vac or pressure oven? Any more information would be much appreciated, Thank You