seanmichaelz
New Member
Have been hammerin blades out now for a couple of months, though new to smithin' wanted to try my hand at forging a layered/damascus billet. Multiple attempts have left me questioning where I am making my mistake? Borax too much, not enough. Am I at forge weld Temp. even though I have the steel coming out almost sparking, To no avail the material wont forge together. So if there is one of you fellas out there could help out a newbie it would certainly go a long way for my sanity and shops' walls... Winters coming!