Search results

  1. Haines Custom

    A couple of Americanized tantos...

    Both look really great.
  2. Haines Custom

    Thoughts on WA Handle finishes

    Does anyone know if this would also work with tung oil?
  3. Haines Custom

    Mosaic Damascus in Black & Blue

    Looks great!
  4. Haines Custom

    How to finish Ultrex Suretouch?

    Appreciate the in formation.
  5. Haines Custom

    Thoughts on WA Handle finishes

    Do you use the ArmorAll on every coat after the first?
  6. Haines Custom

    Jeff Haines pictures

    A2 blade with stabilized hackberry scales and micarta pins. A2 blade with moose scales and micarta pins. Damascus push dagger with fossil walrus handle.
  7. Haines Custom

    How to finish Ultrex Suretouch?

    Thanks for that info.
  8. Haines Custom

    How to finish Ultrex Suretouch?

    I am experimenting with my first suretouch handle on a filet knife. I am wondering about the finishing process. How fine to sand it and what finish, if any, to use. This is intended to be a regular using knife.
  9. Haines Custom

    Field/utility folder

    Very nice.
  10. Haines Custom

    hi from NW Pa.

    Welcome from Wisconsin.
  11. Haines Custom

    Drilling A Wa Handle

    Thanks for the info.
  12. Haines Custom

    3 sheaths

    Nice work.
  13. Haines Custom

    Drilling A Wa Handle

    I apologize for my ignorance but, what is a Wa handle?
  14. Haines Custom

    Stress relief for 15N20 - will it help with warping issues?

    Normalizing won't work for SS in this regard.
  15. Haines Custom

    Stress relief for 15N20 - will it help with warping issues?

    For the 15n20, take it to heat treat temp for 10-15 minutes and air cool.
  16. Haines Custom

    Blades Warping

    For carbide faced hammers you can check out khdailyknives.com . He had some for sale at the last hammer in.
  17. Haines Custom

    Stress relief for 15N20 - will it help with warping issues?

    You might want to consider a normalizing cycle. Per Dr. Larrin Thomas, this should help with warping. The difference is that you heat to austenizing temperature then air cool. His book is a wealth of information but, it gets into a lot of deep science.
  18. Wheel2.jpg

    Wheel2.jpg

    2x2 wheel
Top