7HillsBlade
Member
I have searched around for cryo and LN answers, and haven't found what I was looking for. I am going to utilize this process during the HT of my blades. I will only be doing one blade at a time right now. Just getting started. My questions are:
1. How much LN do you usually buy and how long does it last? 10L, 20L, etc.
2. What type of container do you use to treat your knives with the LN? (do you just use the container the LN is in, or do you have a separate container you use for when treating a blade)
3. How are the blades sitting in the LN? Suspended, etc..
4. How long are you treating the blade? I have seen overnight, and as quick as 30 min. I have CPM-3V at .190 thick.
5. Do you treat it more than once? I have seen multiple and just once.
Thanks guys!!!
1. How much LN do you usually buy and how long does it last? 10L, 20L, etc.
2. What type of container do you use to treat your knives with the LN? (do you just use the container the LN is in, or do you have a separate container you use for when treating a blade)
3. How are the blades sitting in the LN? Suspended, etc..
4. How long are you treating the blade? I have seen overnight, and as quick as 30 min. I have CPM-3V at .190 thick.
5. Do you treat it more than once? I have seen multiple and just once.
Thanks guys!!!