Gene Kimmi
KNIFE MAKER
I'm trying some 1095 for the first time and have a couple questions. I normally grind post heat treat. Is this possible with 1095 since it is a shallow hardening steel, or would I be better off grinding before heat treating? I would also like to try a hamon with this steel. I'm guessing for this it would be better to grind bevels before heat treating? Thanks!
Forgot to say, this is 1/8" material.
Forgot to say, this is 1/8" material.
Last edited: