It's quite possible this has been asked 1,000 times, but here goes. 99% of my knives get sent out to ht, but I'd like to start some experimenting on my own. My research suggests 1084 may be one of the "easier" steels to start with. All I have available at the time for this purpose is a torch. I'd like to do a differential heat treat if possible. Too ambitious? Also how long should I hold the steel at optimal temperature for best results? Also what's the best quencant for this purpose?