HELLGAP
Dealer - Purveyor
I am going to make a hamon line on my next blade. this is what I have, 1084 steel from aldo and the clay I have is RUTLAND REFRACTORY CEMENT it says its good to 2000 f I would like to know should I take a little teaspoon full add a tiny amount of water to make it more runny and then make the wavy line on the blade let it dry and heat treat it. If I dont need to let it dry let me know and if my method is wrong please let me know. Then after I sand it down to 400 then etch and what is the final grit for sanding . I dont know the recipe thanks kellyw